Product Description
Form, roll, mold, texture and even turn this clay on a potter's wheel. Made from a mixture of micron-sized metallic powder, water and organic binder, Prometheus® clay results in a solid metal piece when fired. Because of the high metal content of the powder and binder ratio, pieces are dense and strong to resist cracks or breaks before firing. Longer work time in the wet stage. Must be fired in kiln with activated carbon.
Shrinkage: 6-10%
Firing Temperature: 1420 degrees Fahrenheit (770 degrees Celsius)